Published
Specifies a method for the determination of the ash unplasticized cellulose acetate, free of additives, fillers, dyes or other materials, which may affect the result. -Ignition of a test portion and calcination in a muffle furnace maintained at 575 C or 850 C (as agreed). Higher temperatures such as 850 C will convert carbonates to the oxides and thus give lower values. The general instructions in ISO 3451/1 shall be followed.
PUBLISHED
SSH ISO 3451-3:2009
60.60
Standard published
Jan 1, 2009
Only informative sections of projects are publicly available. To view the full content, you will need to members of the committee. If you are a member, please log in to your account by clicking on the "Log in" button.