Published
ISO 806:2004 specifies a method for the determination of loss of mass on heating of aluminium oxide at 300 °C and further loss of mass on ignition at 1 000 °C. By industry convention, these mass losses are often referred to as "moisture (MOI)" and "loss on ignition (LOI)" respectively.
This method is suitable for calcined alumina in the range 0,2 % to 5 % loss of mass at 300 °C and 0,1 % to 2 % loss of mass at 1 000 °C.
This method provides for samples to be treated on an "as-received" basis for determination of actual MOI and LOI in alumina samples. To improve precision of analysis in cases where "as-received" results are not required, samples can be "air-equilibrated" prior to analysis. "Air-equilibration" can greatly affect MOI results and significantly alter LOI results. The "air-equilibration" procedure and its effects are discussed.
Instrumental methods are also discussed.
PUBLISHED
ISO 806:2004
90.60
Close of review
Sep 3, 2024
Only informative sections of projects are publicly available. To view the full content, you will need to members of the committee. If you are a member, please log in to your account by clicking on the "Log in" button.