ISO 4696-2:2007 specifies a method to provide a relative measure for evaluating the degree of size degradation of iron ores when reduced with carbon monoxide and nitrogen, under conditions resembling those prevailing in the low-temperature reduction zone of a blast furnace.
ISO 4696-2:2007 is applicable to lump ores, sinters and hot-bonded pellets.