Conditioning of 200 parts of plasticiser in the bowl of a planetary mixer at a temperature of 75 C. Addition of 100 parts of the resin to be tested and mixing with the plasticizer. Taking of samples of this mixture at various times, removal of excess of plasticizer by centrifuging and determining the quantity of plasticizer absorbed by the polymer. Plotting a graph, from which can be determined for the polymer under test: - the mean rate of plasticizer absorption (RPA) ; - the hot plasticizer absorption (HPA) at 75 C and 30 min.
WITHDRAWN
ISO 4574:1978
95.99
Withdrawal of Standard
21 maj 2019
PUBLISHED
ISO 4574:2019
Only informative sections of projects are publicly available. To view the full content, you will need to members of the committee. If you are a member, please log in to your account by clicking on the "Log in" button.